What should I do if there are black spots in the granulation of the granulator? In the process of granulation, it is a relatively common problem to encounter black spots on the extracted particles. How to solve this problem? Is this phenomenon caused by the problem of the granulator, the problem of the raw material, or other factors? The following Kelongweier analyze and analyze for everyone.


Black spots in the granulation process are a common failure phenomenon, especially for colored and light-colored products. Often in the final large-scale production process, it is found that the product performance and product color are no problem. However, after a while, I received complaints from customers that "the product qualification rate is too low, there are black spots, request returns" and so on. At this time, the question of why there are black spots has caused many friends to have a headache.


In order to avoid the harm of carbonization to plastic products as much as possible, the key is to prevent effectively and minimize the loss. To deeply understand the nature of carbonization, we must also be good at using effective solutions. We need to strictly control every aspect of solving and preventing the carbonization of plastic products.

Kelongweier Twin screw extruder (1)

To quickly clean the carbides in the machine, you need to use harder plastics or the reclaimed material plus white mineral oil to clean, and the temperature should be appropriately increased by 10~15°C. At this time, the plasticizing ability of the small extruder should be considered. For large and medium-sized extruders that can plasticize ultra-high molecular weight plastics, ultra-high molecular weight plastics or their return materials can be cleaned with white mineral oil. Because ultra-high molecular weight plastics have better hardness, and when the temperature is higher, the cleaning object will be softened and become easy to fall off, which is conducive to the carbide being carried out by the plastic melt. During the cleaning process, the rotation speed of the extruder is repeatedly switched between low speed and high speed many times. If the motor load has a margin, you can repeatedly stop and restart the extruder several times during operation to further improve the cleaning effect. When the carbides (black spots) in the melt are significantly reduced, replace the commonly used plastics and clean them until they are clean, and gradually adjust to the appropriate temperature, then normal production can be performed.


In the actual production of plastic products, the feed inlet is generally isolated before the plastic granulator shuts down to remove the plastic melt in the extruder and die, turn off the temperature of each zone, and then turn off the power. Since the plastic melt has a strong adhesion to the metal, it is impossible to completely eliminate it every time the machine is stopped. In the end, there will always be a thin layer of plastic melt firmly adhered to the barrel and machine of the extruder. On the inner wall of the head and the screw, after the machine is shut down, the equipment will naturally cool down and stay at a high temperature for a long time during the next heating process, which will cause obvious thermal degradation, gradually turn yellow and zoom into carbides. According to the conventional shutdown method, effective sealing measures are not taken at both ends of the die and the feed port of the machine head, which causes air to enter the machine to produce oxidation, which promotes aggravation of the thermal degradation of the residual plastic in the machine, and provides favorable conditions for carbonization.

Kelongweier Twin screw extruder (3)

Because the equipment is a metal structure, its thermal expansion rate is quite different from that of plastic. The adhesion of carbonized plastic to metal is reduced, and it is easy to fall off from the inner wall of the barrel, the inner wall of the head and the screw of the plastic granulator, and it is mixed with the plastic melt. In the body, there are many black spots on the inner and outer walls of the product, which are prone to many quality problems such as piercing or leakage. After a long period of shutdown, heating and restarting, many large and small black spots are prone to appear on the plastic products, which cannot meet the requirements of the product. Quality requirements, these black spots are carbides after thermal deterioration of the residual plastic in the machine. Usually adopt the washing machine method of continuously extruding plastic to eliminate the plastic melt with black spots. The washing time is as long as 3-5 hours. If the original ultra-high molecular weight plastic cup is carbonized and the original color products are produced, it will greatly increase the difficulty of washing the machine, which will make the washing time longer and the washing cost higher.


Kelongweier adheres to the brand belief of "Let technology and art achieve industrial intelligent manufacturing" and the core value concept of "Doing flat double extrusion automation". The core products include parallel twin-screw intelligent equipment, stretch pelletizing, filling, Blending modified water ring eagerly cutting, air-cooled die surface eagerly cutting, underwater pelletizing, continuous mixing and extrusion production line, to provide customers with an overall solution for the intelligent production environment based on rubber and plastic, and is committed to creating high efficiency, energy saving, stability and safety. , Intelligent manufacturing application scenarios.